An fcc iron-carbon alloy initially containing 0.20 wt% c is carburized at an elevated -1 and temperature (semi-infinite diffusion) where the diffusivity is 2 x 10-15 cm2sec in an atmosphere wherein the surface carbon concentration is maintained at 1.1 wt%. at what depth is the carbon concentration equal to 0.3612 wt% if the process time was 24 hours

ansver
Answers: 3

Another question on Chemistry

question
Chemistry, 22.06.2019 01:30
Follow the steps provided in the simulation to add water to the graduated cylinder, select one of the three samples (copper, silver, or gold), set its mass to the values given in the statements below, and calculate its density. here is a summary of the steps required: add water by clicking and holding prepare a known volume of water button. until the desired volume of water has been added. if more than the desired volume is added, click the reset button. button and redo the procedure. a single click will add about 21.0 ml of water. to set the mass, click and hold weigh out metal button. until the desired amount of metal is added to the weighing pan. once the desired mass of the metal is added, release the button. transfer the metal to water and then click on calculate density button. to see how the density is calculated using water displacement to measure the volume of the solid. to save time you can approximate the initial volume of water to â±1 ml and the initial mass of the solid to â±1 g. for example, if you are asked to add 23 ml of water, add between 22 ml and 24 ml. which metals in each of the following sets will have equal density? check all that apply.
Answers: 1
question
Chemistry, 22.06.2019 04:00
Electric charge is what ? a. kinetic energy b. radiation c. discovery d. electricity
Answers: 1
question
Chemistry, 22.06.2019 05:40
Can someone me with 1 to 4 plz. fast
Answers: 1
question
Chemistry, 22.06.2019 10:10
Stage in which a star’s outer layers have started to cool and grow outward?
Answers: 3
You know the right answer?
An fcc iron-carbon alloy initially containing 0.20 wt% c is carburized at an elevated -1 and tempera...
Questions
Questions on the website: 13722359