For a steel alloy it has been determined that a carburizing heat treatment of 11.3 h duration will raise the carbon concentration to 0.44 wt% at a point 1.8 mm from the surface. Estimate the time necessary to achieve the same concentration at a 4.9 mm position for an identical steel and at the same carburizing temperature.

ansver
Answers: 1

Another question on Engineering

question
Engineering, 04.07.2019 16:10
The force on a cutting tool are 2600n vertically downward and 2100 horizontal. determine the resultant force acting on the tool and the angle at which it acts.
Answers: 1
question
Engineering, 04.07.2019 18:10
Acompressor receives the shaft work to decrease the pressure of the fluid. a)- true b)- false
Answers: 3
question
Engineering, 04.07.2019 18:10
Manometers are good examples of measuring instruments, nowadays they are not as common as before. a)-capacitive probe gauges b)-gravitational gauges deformation ) gauges d)-digital gauges
Answers: 1
question
Engineering, 04.07.2019 18:20
Prove the equivalence between the two statements of the 2nd law of thermodynamics (i.e., a violation of one statement leads to the violatio the other statement)
Answers: 2
You know the right answer?
For a steel alloy it has been determined that a carburizing heat treatment of 11.3 h duration will r...
Questions
question
Mathematics, 13.11.2020 01:00
question
Mathematics, 13.11.2020 01:00
question
Biology, 13.11.2020 01:00
question
Computers and Technology, 13.11.2020 01:00
question
Mathematics, 13.11.2020 01:00
Questions on the website: 13722367